Coating properties | Influence of Process Conditions | Effect of bath composition |
Tensile stress | When the temperature of the plating solution is lower than 49°C, it decreases with the increase of the temperature of the plating solution, and when the temperature of the plating solution is above 49°C, it increases slowly with the increase of the temperature Increase with the increase of bath pH Decreases with increasing cathode current density | Decrease slightly with increasing nickel content |
Elongation | When the bath temperature is 43°C, it reaches the maximum value Decrease with the increase of bath pH Increased with the increase of cathode current density | Slightly increased with the increase of nickel content Slightly increased with the increase of chloride content |
hardness | In the process range, it increases with the increase of temperature Increase with the increase of bath pH When the cathode current density is about 13A/dm3, it reaches the lowest value | Decrease slightly with the increase of Ni2+ concentration Slightly decreased with the increase of chloride content |
Internal stress | Decreases with increasing bath temperature When the pH of the plating solution is 4.0-4.2, it reaches the lowest value increases with the increase of cathode current density Within the specified pH range, it will not be affected by pH changes | Within the process range, the change of Ni2+ content in the bath has little effect on it significantly increased with the increase of chloride content |
刘宏宇; 张松 - 《有机硅耐高温涂料的研制》
戴英才 - 《涂料检验方法标准浅谈》