Back
Knowledge

ASTM D2240 Rubber Properties, Hardness Tester Hardness Testing

Abstract: 文章介绍了 ASTM D2240 硬度计硬度测试方法,该方法用于测量材料中压痕的深度,以评估其硬度。硬度与材料的延展性和压头形状成正比,常用于复合材料和聚合物的测试。文章还强调了 ASTM D2240 测试中的关键因素,如初始硬度、样品形状、硬度计类型以及测试条件。测试通常在 23 ± 2 °C 和 50±5% 相对湿度下进行,要求样品平坦且无纹理,并使用“A”和“D”刻度的硬度计进行测量。

ASTM D2240 – Durometer Hardness is a test method designed to measure the depth of an indentation in a material being tested. Indentations are produced with a given force on a standard indentation head. Depth is proportional to the hardness of the material (also known as Shore hardness), its ductility and the shape of the indenter. ASTM D2240 uses rubber properties and durometer hardness and involves pressing the indentation head on the bottom of the hand-held device until the flat bottom part rests on the surface of the material to be tested.


This test method is widely used in composite materials and polymer testing.


ASTM D2240 Uses and Factors to Consider

ASTM D2240 allows the measurement of initial hardness or indentation hardness after a given time. This test requires force to be applied in a consistent manner, without impact, and hardness is measured. There are 12 scales, and there is no mathematical relationship between the various scales because they are arbitrary scales. Therefore, it is important to know which scale you need for your lab.


ASTM D2240 Typical Test Parameters

Initial Hardness or Timed Hardness: Usually Initial Hardness

Specimen shape: flat and homogeneous (no texture)

Durometers to use: The mainstream durometers are "A" and "D". Together, the two scales cover a range of durometers from rubber to nylon.

Number of samples per product: 1 sample, 5 readings

Sample size: 2” X 2” or larger with a minimum thickness of 6.4 mm (0.25 in.) thick.

Conditioning and testing temperature: 23 ± 2 °C

Conditioning and testing relative humidity: 50±5%


Relevant knowledge
Guess you like it