United States

US RDS 3 #3/8 "Mayer Rods coating bar 6.9μm Length 400mm

SE
Mayer principle is the thinnest steel wire in RDS bar and the thinnest model of wire-wound film. It is also one of the best-selling models of RDS and is deeply loved by Testers.
$161.00/piece
PromotionLoading...
Coupon
Model:

RDS 3# 3/8 Applicator rod 3/8SPEC

RDS 3# 3/8 Applicator rod 3/8Details

RDS 3# 3/8 Applicator rod 3/8Packing list

SKU
NB000001
Production process
wire-wound
WFT
6.9μm
diameter
9.52mm
Total length
400mm
application width
300mm
Grip Width
50+50mm
material
stainless steel
Wire diameter
0.08mm
3# 3/8
Applicator rod 3/8
Mayer principle is the thinnest steel wire in RDS bar and the thinnest model of wire-wound film. It is also one of the best-selling models of RDS and is deeply loved by Testers.
US RDS 3 #3/8 "Mayer Rods coating bar 6.9μm Length 400mm Picture

RDS coating Rods Figure 1

RDS coating Rods Figure 2

RDS coating Rods Figure 3

RDS coating Rods Figure 4

RDS coating Rods Figure 5

RDS coating Rods Figure 6

RDS coating Rods Figure 7

RDS coating Rods Figure 8

RDS coating Rods Figure 9

RDS coating Rods Figure 10


FAQ
QApplicator rods preparing approximately 7 micron coatings, which model should be selected?
A Recommended RDS No. 3 Mayer Rods, model 3 #3/8. This coating applicator is specifically designed for the preparation of wet-film coatings of approximately 7 μm (actual wet film thickness is 6.9 μm), suitable for precision film thickness control in Coatings, inks and most fluid industries, ensuring Spreader accuracy and conformity.
QWhich Applicator rod is suitable for hard substrates?
A It is recommended to choose a molding coating rod with a diameter of 6.35mm (a model of RDS No. 3 rod). The reason for the recommendation is that the molding rod adopts an integrated molding process and has no winding steel wire structure, which can avoid the problem of broken wire caused by improper cleaning, bumping or hard substrate Spreader (the probability of broken wire is only 0.2%). It is more suitable for users with high environmental requirements or worried about accidental damage.
QPreparative 2D single crystal copper nanosheet films can be coated with bar?
A Yes, Mayer Rods (Mayer-Rod) can prepare 2D single crystal copper nanosheet films by electrochemistry and has good shape control and application potential.
QCan RDS3 rod be scraped with lithium battery paste?
A Yes, the film thickness of RDS is 6.9 microns.
QHow thick is the paint film scraped out by No. 3?
A wet-film 6.9um, dry-film thickness depends on your solid content
QUsed in diaphragm Spreader, slurry solid content of 30%, viscosity of about 300cp, want to prepare Dry-Film 2 micron, 5-6 micron coating, how much wet film thickness is better
A Recommend stick No. 3.
QHow to clean RDS Mayer Rods?
A Mayer Rods cleaning is divided into three steps: 1. Soak it in a suitable solvent; 2. Rinse it with water; 3. After cleaning, air dry or dry it and put it in the rod cartridge.
QIs Mayer Rods No. 3 the smallest stick size?
A No, the Grooved Rods of rds also have sticks 2 and 0.
QHow many microns is the thinnest RDS Mayer Rods wide-wound?
A 6.9 microns, if the forming rod can be scraped to 4.6 μm.
QHow much wet do you apply to rds3?
A Wet film thickness 6.9μm.
Knowledge
Standard