China

ZHANYI No. 6 Mayer Rods film thickness 6μm Total length 240mm

SE
Formed, wet film thickness 6μm, diameter 10mm, Total length 400mm, application width 205mm, hand width 17.5 + 17.5mm, material stainless steel.
Model:
Certificate

ZhanYi ZY-6/240 Mayer RodsSPEC

ZhanYi ZY-6/240 Mayer RodsDetails

ZhanYi ZY-6/240 Mayer RodsPacking list

SKU
NB000189
Production process
Formed
WFT
6μm
diameter
10mm
Total length
400mm
Application width
205mm
Grip width
17.5+17.5mm
material
stainless steel
ZY-6/240
Mayer Rods
Formed, wet film thickness 6μm, diameter 10mm, Total length 400mm, application width 205mm, hand width 17.5 + 17.5mm, material stainless steel.
ZHANYI No. 6 Mayer Rods film thickness 6μm Total length 240mm Picture

The domestic (CN) Zhanyi wire rod coater is an extruded coating rod, which is carefully developed by integrating domestic (CN) and foreign professional technologies and can coat wire with the same effect as the wire-wound coating rod without wire winding. Rod coater, No. 6 wire rod coater has a coating film thickness of 6 microns and has two lengths of 240mm and 400mm. It is very suitable for preparing samples of specific wet film thickness in the laboratory, and measuring the hiding power, color and luster of the coating film. Drying time and other properties are widely used in paint, paint, ink and other industries.

Zhanyi No.6 wire rod coater operation video

Zhanyi No.6 wire Bar Coater specifications

Features and advantages of Zhanyi No. 6 wire rod coater

Zhanyi No. 6 wire rod coater Applications

Zhanyi No. 6 Wire Rod Coater Real Shot Figure 1

Zhanyi No. 6 Wire Rod Coater Real Shot Figure 2

Optional

Experimental coating test cardboard

Imprint bed coating station

LABOratory small automatic film coating machine

FAQ
QHelp me find a Mayer Rods that meets the GB/T26461 standard.
A This ZY-6/240 Mayer Rods is fine!
QCan this scraper be used to coat organic polymer conductive films?
A Yes, the specific selection can be selected by the appropriate rod number corresponding to the rod model and film thickness, by optimizing a series of factors such as wet film thickness, Spreader speed, surfactant concentration, ethylene glycol concentration, film heat treatment temperature, etc., so that It is worth the conductive film compound requirements.
QCan silicone coatings be applied to quartz Glass substrates?
A Yes, choose quartz Glass as the substrate, with Mayer Rods Coating prepared above coated on the surface of the treated quartz Glass substrate, at room temperature to evaporate the solvent into the oven, at a certain temperature curing film formation.
Q6 #What is the thickness of the Spreader Film?
A Hello, different brands of 6 #Spreader sticks correspond to different Spreader Film thicknesses. The No. 6 wire rod of RDS is 13.7 μm; the No. 6 wire rod of RK is 60 μm; the No. 6 wire rod of OSP and Spreader, modern is 6 μm.
QWhat number of Mayer Rods is generally used for Gloss oil testing?
A Mayer Rods is used by many companies, from a few microns to hundreds of microns. So it also needs to be calculated based on the wet film thickness you want to scrape.
QCan this domestic (CN) Mayer Rods paint a uniform film 6 microns thick?
A The domestic (CN) Mayer Rods is used to prepare a specific wet film of 6μm, please ensure that the Spreader platform is flat, the levelling performance has a certain relationship with your hand scraping, and more importantly, the influence of your Spreader fluid on the levelling performance.
QI want to apply glue, about 10cm. I'm not sure how thick to apply it. How to choose?
A It is recommended that you calculate the wet film thickness according to NBchao's wet film thickness calculator.
QSolid content of the sample is 40%, Dry-Film needs 2 microns, do you have any suggestions?
A This one is fine.
Standard