China

ZHANYI No. 8 Mayer Rods Total length 240mm application width 205mm

SE
Formed, wet film thickness 8μm, diameter 10mm, Total length 240mm, application width 205mm, hand width 17.5 + 17.5mm, material stainless steel.
Model:
Certificate

ZhanYi ZY-8/240 Mayer RodsSPEC

ZhanYi ZY-8/240 Mayer RodsDetails

ZhanYi ZY-8/240 Mayer RodsPacking list

SKU
NB000190
Production process
Formed
WFT
8µm
diameter
10mm
Total length
240mm
Application width
205mm
Grip width
17.5+17.5mm
material
stainless steel
ZY-8/240
Mayer Rods
Formed, wet film thickness 8μm, diameter 10mm, Total length 240mm, application width 205mm, hand width 17.5 + 17.5mm, material stainless steel.
ZHANYI No. 8 Mayer Rods Total length 240mm application width 205mm Picture

Zhanyi No. 8 wire rod coater can prepare a film thickness of 8 μm. It is a one-frame extrusion type, not easy to break, not easy to rust, and a very affordable domestic (CN) wire rod coater. It can be widely used in the coating and ink industry. , with the introduction of NBCHAO Mall, the influence of Zhanyi wire rod coater in CHINA has gradually increased. The specific introduction can be seen in the following detailed introduction:

Zhanyi No.8 wire rod coater operation video

Specifications of Zhanyi No.8 Wire Bar Coater

Features and advantages of Zhanyi No. 8 wire rod coater

Zhanyi No.8 wire rod coater Applications

Zhanyi No. 8 Wire Rod Coater Real Shot Figure 1

Zhanyi No. 8 wire rod coater real shot picture 2

Optional

Experimental coating test cardboard

Imprint bed coating station

LABOratory small automatic film coating machine

FAQ
QCoating rod domestic (CN) is not less than 10mm, film Film thickness 2.5um model?
A Hello, no, there is currently no domestic (CN) rod that can achieve such a thick film. You can consider OSP's L60 rod.
QMy percent solids are 16 percent, and I want to apply Dry-Film 1 micron. Can this stick do it?
A Sure
QCan this coating rod be prepative of multi-layer ultra-thin film?
A The wire rod can be prepared for 1.5 micron ultra-thin film. Everyone must know it, but another advantage of it is multi-layer film, which is much better than I-shaped film applicator. But multi-layer film tests the flatness of the previous layers of film drying. Generally, the film thickness (such as less than 10 microns/layer) is too thin to control. The wire rod with Film Applicator is a very good solution, eliminating the problem of uneven pressure and speed of hand scraping.
QDoes Mayer Rods meet the specifications of GB/T26461?
A Model ZY-8/240 Mayer Rods Compliant
QHow to use this domestic (CN) Mayer Rods? Is there a video tutorial?
Standard