30, 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46, 47, 48, 49, 50, 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62, 63, 64, 65, 66, 67, 68, 69, 70, 72
Built-in 15ml test solution, which can be used more than 100 times
6-8 months shelf life
The tip of the pen is carefully designed to reduce the chance of contact between dyne liquid and air
Each pen has been inspected many times, quality assurance
Strictly comply with ASTM Standard D2578 standard and TAPPI T698 standard
It can accurately test whether the surface tension of the plastic film reaches the value of the test pen. Let users know clearly whether the film is suitable for printing, lamination or vacuum aluminum plating, etc., so as to effectively control the quality and reduce the loss caused by unqualified materials. It is not limited to plastic films, but can also test the surface tension of various materials.
| printing process | other process | ||||||||||||||||||
| process | Flexo and Gravure | lithograph | Offset / Letterpress | Screen Printing and Pad Printing | laminated | Coating, coating | |||||||||||||
| coating type | watermark | solvent | UV | watermark | solvent | UV | watermark | solvent | UV | watermark | solvent | UV | watermark | solvent | UV | watermark | solvent | UV | |
| matrix | Polyethylene ( PE) | 38 | 36 | 38 | 40 | 37 | 40 | 40 | 37 | 42 | 42 | 38 | 44 | 42 | 38 | 42 | 42 | 38 | 44 |
| 44 | 40 | 50 | 46 | 42 | 50 | 46 | 42 | 54 | 48 | 44 | 60 | 50 | 44 | 54 | 48 | 45 | 54 | ||
| Polypropylene (PP) | 38 | 36 | 40 | 40 | 38 | 40 | 40 | 37 | 40 | 42 | 38 | 44 | 42 | 38 | 42 | 42 | 38 | 44 | |
| 44 | 40 | 50 | 46 | 42 | 50 | 46 | 42 | 54 | 48 | 44 | 60 | 50 | 44 | 54 | 48 | 45 | 54 | ||
| Polyvinyl chloride (PVC) | 38 | 36 | 36 | 40 | 37 | 36 | 40 | 38 | 40 | 42 | 38 | 42 | 42 | 38 | 42 | 40 | 38 | 42 | |
| 44 | 40 | 50 | 45 | 42 | 52 | 45 | 42 | 52 | 48 | 44 | 60 | 50 | 44 | 54 | 48 | 45 | 54 | ||
| Polyethylene terephthalate (PET) | 44 | 40 | 42 | 46 | 42 | 44 | 46 | 42 | 46 | 48 | 42 | 44 | 46 | 42 | 44 | 42 | 42 | 46 | |
| 52 | 46 | 54 | 56 | 46 | 56 | 56 | 46 | 60 | 60 | 48 | 62 | 60 | 48 | 62 | 52 | 48 | 60 | ||
| Polystyrene (PS) | 38 | 35 | 42 | 40 | 37 | 42 | 40 | 38 | 42 | 42 | 38 | 42 | 42 | 37 | 42 | 42 | 38 | 44 | |
| 44 | 40 | 48 | 45 | 42 | 50 | 46 | 44 | 58 | 48 | 44 | 56 | 52 | 44 | 54 | 50 | 46 | 54 | ||
| Polyvinylidene Chloride (PVDC) | 40 | 38 | 42 | 42 | 40 | 42 | 42 | 38 | 42 | 42 | 40 | 42 | 42 | 38 | 44 | 42 | 40 | 44 | |
| 46 | 42 | 52 | 46 | 42 | 52 | 48 | 44 | 54 | 50 | 45 | 58 | 50 | 44 | 52 | 48 | 46 | 54 | ||
| Polyurethane (PU) | 40 | 38 | 38 | 40 | 38 | 38 | 40 | 38 | 42 | 42 | 38 | 42 | 42 | 38 | 42 | 42 | 38 | 44 | |
| 46 | 42 | 50 | 46 | 42 | 52 | 45 | 44 | 56 | 50 | 44 | 58 | 50 | 44 | 56 | 48 | 46 | 54 | ||
| Acrylonitrile - butadiene - styrene (ABS) | 42 | 40 | 40 | 42 | 40 | 42 | 42 | 38 | 45 | 42 | 40 | 46 | 42 | 40 | 42 | 42 | 38 | 44 | |
| 46 | 44 | 52 | 46 | 45 | 52 | 48 | 46 | 52 | 48 | 45 | 56 | 52 | 45 | 56 | 48 | 46 | 54 | ||
| Polytetrafluoroethylene (PTFE) | 40 | 34 | 36 | 40 | 35 | 38 | 40 | 38 | 42 | 42 | 38 | 42 | 42 | 38 | 42 | 42 | 40 | 42 | |
| 44 | 39 | 52 | 45 | 40 | 52 | 48 | 44 | 60 | 52 | 46 | 60 | 56 | 46 | 56 | 50 | 48 | 54 | ||
| Silicone | 40 | 35 | 40 | 40 | 38 | 38 | 40 | 38 | 40 | 42 | 38 | 42 | 42 | 38 | 42 | 42 | 40 | 42 | |
| 44 | 40 | 50 | 45 | 42 | 52 | 48 | 44 | 56 | 50 | 46 | 60 | 56 | 46 | 56 | 50 | 48 | 54 | ||
Plastic films: PS, PE, PP, PET, PI, PC, NY, CPP, OPP, PVC,
Conductive materials: aluminum foil, copper foil, carbon foil, evaporated film.
Other materials: glass, ceramics, plastic sheets, plastic pipes, etc.
Choose a corona pen with a suitable dyne value
Clean the surface of the film and lay it flat on a horizontal table
Gently draw a stroke on the film surface with a corona pen
If the fluid does not shrink within three seconds, the selected dyne is reached, otherwise not.