China

MODERNER XB-20 bar WFT 20μm

The MODERNER XB-20 wire rod is a wire-wound stainless steel wire rod with a film thickness of 20μm, and the application width of the CHINA paint rod Applicator is 200mm.
Model:
Certificate

Moderner XB-20 Mayer RodsSPEC

Moderner XB-20 Mayer RodsDetails

Moderner XB-20 Mayer RodsPacking list

SKU
NB004548
Production process
Wire-wound
WFT
20μm
Total length
240mm
Application width
200mm
grip width
20+20mm
material
stainless steel
XB-20
Mayer Rods
MODERNER XB-20 bar WFT 20μm Picture

Introduction to XB-20 wire rod

Modern Environment XB-20 wire rod has a coating thickness of 20 microns, a wire-wound stainless steel wire rod with a rod length of 240mm, and a coating width of 200mm. Made of corrosion-resistant stainless steel, it has good corrosion resistance. MODERNER XB series wire rod applicator can be used with a handle (need to be purchased separately), making coating easier and more effective.

Specifications

modelXB-7XB-10XB-12XB-15XB-20XB-25XB-30XB-40XB-50XB-60XB-80XB-100XB-120XB-150XB-200XB-250XB-300
Wet film thickness (μm)710121520253040506080100120150200250300
Total length (mm)240240240240240240240240240240240240240240240240240
Coating width (mm)200200200200200200200200200200200200200200200200200

Note: XB wire rod applicator needs to purchase an additional handle

Instructions

First, place the sample on the platform and fix it to ensure that the sample cannot move when the XB coating scraper passes over it.

Second, select the appropriate XB coating scraper according to the required wet film thickness and place it at the position specified on the sample.

Third, pour an appropriate sample in front of the xb coating scraper, hold the handle (need to be purchased separately) with your hand, and slide it at a constant speed of 150 mm/second, that is, apply a wet film with the required thickness.

Note: The XB coating scraper must be washed and dried with an appropriate solvent immediately after use to prevent the paint from drying out after too long and making it difficult to clean, causing blockage and affecting subsequent experiments.

Product actual pictures

MODERNER XB-20 wire rod WFT 20μm real shot picture 01

MODERNER XB-20 wire rod WFT 20μm real shot picture 02

MODERNER XB-20 wire rod WFT 20μm real shot picture 03

MODERNER XB-20 wire rod WFT 20μm real shot picture 04

Optional

Experimental coating test paper

Imprint bed coating station

Laboratory small automatic film coating machine