| fit system | Ternary, lithium iron phosphoric acid, lithium cobaltate, lithium manganate, graphite, silicon carbon and other systems of batteries positive and cathode sheet Spreader process |
| Coating method | Continuous Spreader, Intermittent Spreader |
| Film thickness of running substrate | Aluminum foil (Al): 8~ 30um; Copper foil (Cu): 6~ 30um |
| Roller surface design width | 300 mm |
| Guaranteed Spreader Width | Within 240mm |
| main roller | Φ150mm |
| Spreader Accuracy | ±1.5um |
| Suitable slurry viscosity | 2000~12000 (mPas) |
| Film thickness range of single top coating | 10-250μm |
| Solvent characteristics | Oily solvent NMP (s.g = 1.033, b.p = 204 ℃); aqueous solvent H2O/NMP (s.g = 1.000, b.p = 100 ℃) |
| Solid content range | 20~85% |
| Spreader dimensional Accuracy | L≤±1mm、W≤±0.4mm |
| Front and back alignment Accuracy | L≤±1mm、W≤±0.4mm |