China

QAG-2 levelling Tester YONGLIDA 100~1000μm WFT

SE
Coating range 100~1000μm; Dimension groove 120 * 22 * 20mm; stainless steel material; in line with ASTM/D2801, JB/T3998 standards.
$148.00/piece
PromotionLoading...
Coupon
Model:
Certificate

YongLiDa QAG-2 Leveling TesterSPEC

YongLiDa QAG-2 Leveling TesterDetails

YongLiDa QAG-2 Leveling TesterPacking list

SKU
NB002804
groove depth
100-200-300-500-1000μm
Overall Dimensions
120*22*20mm
QAG-2
Leveling Tester
Coating range 100~1000μm; Dimension groove 120 * 22 * 20mm; stainless steel material; in line with ASTM/D2801, JB/T3998 standards.
QAG-2 levelling Tester YONGLIDA 100~1000μm WFT Picture

Introduction of QAG-2 Leveling Applicator

Yonglida QAG-2 Leveling Applicator is used to test the relative leveling of liquid coatings in the laboratory, that is, the ability of coatings to eliminate surface defects during the drying process. The coating thickness of QAG-2 Leveling Applicator is 250~400μm, which complies with the international standard ASTM D2801 and JB/T3998-1999.

plan

Yonglida QAG-2 Leveling Tester Details Figure 1

FAQ
Q3998-1999 Satisfied? [YONGLIDA] QAG-2 leveling tester
A This can satisfy
QWhat is the wet film thickness tested by Yonglida AG-2 levelling tester?
A Hello, the wet film thickness is 250~ 4000 μm.
QI want to do a test on the ASTMD 4062-99 standard. Is this leveling tester okay?
A Sure
Knowledge